Behavior of Rp3-High Spped on Short Time Nitriding in Fluidized Bed
Fecha
2005Autor
Bâclea, Adolf
Cazacu, Nelu
Dobrovici, Sorin
Drugescu, Elena
Potecașu, Octavian
Metadatos
Mostrar el registro completo del ítemResumen
For steel nitriding, treatment time is a important factor. Gas and plasma
nitriding are usual method to increase surface properties by nitriding. A close
retort is used. Total time for treatment are higher because are necessary transition
time for heating and cooling. Fluidized bed offer a short time for heating and
cooling because furnace having an open retort. Work paper is based by nitriding
experiments by experimental fluidized bed furnace. A gas mixture of ammonia and
nitrogen was used. For samples were used HHS (Rp3) . Results were investigated
micrographic, surface hardness test (HV5) and micro hardness (HV0,05).